Volume 39 (2024-2025)
Volume 38 (2023-2024)
Volume 37 (2022-2023)
Volume 36 (2021-2022)
Volume 35 (2020-2021)
Volume 34 (2019-2020)
Volume 33 (2018-2019)
Volume 32 (2017-2018)
Volume 31 (2016-2017)
Volume 30 (2015-2016)
Volume 29 (2014-2015)
Volume 28 (2013-2014)
Volume 27 (2012-2013)
Volume 26 (2011-2012)
Volume 25 (2010-2011)
Volume 24 (2009-2010)
Volume 23 (2008-2009)
Volume 22 (2007-2008)
Volume 21 (2006-2007)
Volume 20 (2005-2006)
Volume 19 (2004-2005)
Volume 18 (2003-2004)
Volume 17 (2002-2003)
Volume 16 (2002-2003)
Volume 15 (2001-2002)
Volume 14 (2001-2002)
Volume 13 (2001)
Volume 12 (2000-2001)
Volume 11 (2000-2001)
Volume 10 (2000-2001)
Volume 9 (2000)
Volume 8 (1999)
Volume 7 (1999)
Volume 6 (1998)
Volume 5 (1998)
Volume 4 (1997)
Volume 3 (1997)
Volume 2 (1996)
Volume 1 (1995)
Author = Tabarsa, Taghi
Number of Articles: 4
The manufacture of particleboard using tannin-modified urea formaldehyde adhesive
Volume 28, Summer 2 , June 2013, , Pages 266-276
Abstract
This study provides an investigation of particleboard manufacture using tannin-ureaformaldehyde adhesive. Test board samples were made with regard to various replacementpercentage of tannin–urea (levels of 0, 10, 20 and 30%) and press time (12 and 15 min) andtheir properties were determined. Achieved ... Read MoreThe manufacture of particleboard using mixture of golestan province wheat straw and cotton bolls reinforced with nano-clay particles
Volume 28, Summer 2 , June 2013, , Pages 277-289
Abstract
In this study, Wheat straw particle boards were produced using a mixture of wheat straw andcotton bolls with Urea formaldehyde resin and its properties were reinforced with nanoclay.Cotton bolls and wheat straw particles were mixed at the ratio of 40:60, 60:40 and 80:20percents, respectively. Nanoclay ... Read MoreThe effects of thermal treatment and resin type on physical and mechanical properties of Kenaf stalk particleboard
Volume 28, Summer 2 , June 2013, , Pages 313-328
Abstract
The objective of this study was to manufacture water resistant kenaf stalk particleboard.Twenty seven boards were produced using 170 °C steam treated kenaf particles, 30 and 60minute treatment time and three resin types include urea-formaldehyde, melamineformaldehydeand a mixture of fifty percent ... Read MoreConstruction of Particlboard Using Tannin-Based Phenol Adhesive