@article { author = {Ibaghi esfahani, Hamid and Kalagar, Mehdi and Sepehridad, Hossein}, title = {The effect of elastomers and coupling agent on tensile properties and impact strength polypropylene/saw dust composites}, journal = {Iranian Journal of Wood and Paper Science Research}, volume = {32}, number = {2}, pages = {157-170}, year = {2017}, publisher = {Research Institute of Forests and Rangelands}, issn = {1735-0913}, eissn = {2383-112X}, doi = {10.22092/ijwpr.2017.109584}, abstract = {To study the tensile properties and impact strength in Wood Plastic Composites (WPC) polypropylene as a matrix and teada pine sawdust as reinforcement / filler is used. Ethylene / propylene / Diane / monomer (EPDM) as modified impact resistance with 10, 20 and 30 percent improved impact resistance and maleic anhydride grafted polypropylene (MAPP) at a rate of 3 percent as a fasteners to improve response and polymers and fillers were added to the composite. To evaluate the fracture surface of a structure scanning electron microscope (SEM) was used. The apply of 10 % elastomer and 3 % coupling agent cause to improved of tensile properties and the use of higher levels of elastomer (20 and 30 %) has shown a decreasing trend in these properties. The results showed that PP matrix by adding sawdust to a significant reduction in impact strength of composite than pure PP is observed. An EPDM additive used in all contents of composites PP / sawdust has improved impact strength. Simultaneous use of EPDM and MAPP used a positive effect in tensile properties and impact strength. The apply of EPDM (30%) and 3% (MAPP) has demonstrated the highest level of impact strength. SEM images show that the use of EPDM and MAPP composites will improve the connection of interface.}, keywords = {Composite,tensile properties,impact strength,Ethylene / propylene / Diane / monomer,Coupling agent}, title_fa = {تاثیر الاستومر و اتصال دهنده بر ویژگی های کششی و مقاومت به ضربه چندسازه پلی پروپیلن/ خاک اره}, abstract_fa = {جهت بررسی ویژگی‌های کششی و مقاومت به ضربه در چندسازه چوب پلاستیک (WPC) از پلی پروپیلن به عنوان ماتریس و خاک اره کاج تدا به عنوان تقویت کننده/ پرکننده استفاده شده است. اتیلن/ پروپیلن/ داین/ منومر (EPDM) به عنوان اصلاح کننده مقاومت به ضربه با میزان های 10، 20 و 30 درصد جهت بهبود مقاومت به ضربه و انیدرید مالئیک پیوند خورده با پلی پروپیلن (MAPP) به میزان 3 درصد به عنوان اتصال دهنده جهت بهبود واکنش و اتصال پلیمر و پرکننده به ترکیب چندسازه اضافه شدند. جهت بررسی سطح شکست در چندسازه از میکروسکوب الکترونی پوبشی (SEM) استفاده شد. به کارگیری 10 درصد الاستومر و 3 درصد اتصال دهنده باعث بهبود در ویژگی‌های کششی شده و استفاده از میزان‌های بالاتر الاستومر (20 و 30 درصد) روند کاهشی در این ویژگی‌ها را نشان داده است. نتایج نشان داد که با افزودن خاک اره به ماتریس PP کاهش قابل توجه‌ای در مقاومت به ضربه چدسازه نسبت به PP خالص مشاهده شده است. افزودن EPDM در تمامی میزان های مورد استفاده به چندسازه PP/ خاک اره باعث بهبود در مقاومت به ضربه چندسازه شده است. بالاترین مقادیر مقاومت به ضربه متعلق به چندسازه حاوی 30 درصد الاستومر و 3 درصد اتصال دهنده بوده است. استفاده همزمان از EPDM و MAPP تاثیر مثبتی بر ویژگی‌های کششی و مقاومت به ضربه چندسازه را نشان داده است. تصاویر SEM نشان داده که استفاده همزمان از EPDM و MAPP در چندسازه باعث اتصال سطح مشترک بهتر خواهد شد.}, keywords_fa = {چندسازه,ویژگی‌های کششی,مقاومت به ضربه,اتیلن/ پروپیلن/ داین/ منومر,اتصال دهنده}, url = {https://ijwpr.areeo.ac.ir/article_109584.html}, eprint = {https://ijwpr.areeo.ac.ir/article_109584_d363ac571d57035767eff84bb09eb938.pdf} } @article { author = {Dalvand, Mosayeb and Ebrahimi, Ghanbar and Pourtahmasi, Kambiz}, title = {Investigation on withdrawal capacity of staple in the upholstered furniture frame made of LVL}, journal = {Iranian Journal of Wood and Paper Science Research}, volume = {32}, number = {2}, pages = {171-180}, year = {2017}, publisher = {Research Institute of Forests and Rangelands}, issn = {1735-0913}, eissn = {2383-112X}, doi = {10.22092/ijwpr.2017.109762}, abstract = {In this study effect of staple length (penetration length) and its number in connection, on withdrawal capacity in face and edge of laminated veneer lumber (LVL) out of poplar was investigated. In this investigation, the staple with 3 and 4 cm penetration length and staple with 3, 4 and 5 cm penetration length for withdrawal capacity in face and edge were used respectively. Number of staples at 4 levels (2, 3, 4 and 5) were chosen as a variable. Results have shown that withdrawal capacity in face significantly increases with increase of penetration length. Withdrawal capacity in edge increases drastically with increase of penetration length from 3 to 4 cm, but increase in penetration length from 4 to 5 cm had no significant effect. Withdrawal strength capacity in face has increased with increase of staples number. But, increase of staple number had no significant effect on withdrawal strength capacity in edge. Maximum withdrawal capacity was observed in joints fabricated with penetration length of staple 4 cm and number of 5 staples in face and minimum those were observed with penetration length 3 cm and number of 2 staples in edge.}, keywords = {Withdrawal strength capacity,Upholstered furniture,Staple,LAMINATED VENEER LUMBER}, title_fa = {بررسی ظرفیت نیروی انفصال اتصال با منگنه در قاب مبلمان راحتی از LVL}, abstract_fa = {در این پژوهش تاثیر طول پایه (طول نفوذ) منگنه و تعداد آن بر ظرفیت نیروی انفصال منگنه در سطح و لبه چند سازه لایه‌ای (LVL) ساخته شده از گونه صنوبر مورد بررسی قرار گرفته است. در این بررسی برای آزمون ظرفیت نیروی انفصال منگنه در سطح از منگنه با طول نفوذ 3 و 4 سانتی‌متری و برای آزمون ظرفیت نیروی انفصال لبه از منگنه با طول نفوذ 3، 4 و 5 سانتی‌متری استفاده شده است. تعداد منگنه در 4 سطح (2، 3، 4 و 5 عدد) برای هر دو آزمون به عنوان متغیر انتخاب شد. نتایج نشان داده‌اند که با افزایش طول نفوذ منگنه ظرفیت نیروی انفصال منگنه در سطح به طور محسوسی افزایش پیدا می‌کند. ظرفیت انفصال منگنه در لبه LVL با افزایش طول نفوذ از 3 به 4 سانتی‌متر روند صعودی دارد ولی این روند از طول نفوذ 4 به 5 سانتی‌متری نامحسوس است. ظرفیت نیروی انفصال منگنه در سطح با افزایش تعداد اتصال دهنده افزایش داشته،. ولی تعداد منگنه در ظرفیت نیروی انفصال منگنه در لبه LVL تاثیر معنی‌داری نداشت. بیشترین ظرفیت انفصال منگنه در سطح، مربوط به اتصال‌های ساخته شده از منگنه با طول نفوذ 4 سانتی‌متر با تعداد 5 منگنه بوده است و کمترین آن در لبه، مربوط به طول نفوذ 3 سانتی متر و تعداد 2 منگنه بوده است.}, keywords_fa = {ظرفیت نیروی انفصال,مبلمان راحتی,منگنه,چند سازه لایه ای}, url = {https://ijwpr.areeo.ac.ir/article_109762.html}, eprint = {https://ijwpr.areeo.ac.ir/article_109762_33786010f1951e0f72f15bf0ebaed75c.pdf} } @article { author = {Porbar, Samira and Hosseinzadeh, Omid and Hajjarian, Marzieh}, title = {Prioritize of poplar wood processing industries in the Kurdistan province with the aim of poplar wood value chain upgrading}, journal = {Iranian Journal of Wood and Paper Science Research}, volume = {32}, number = {2}, pages = {181-192}, year = {2017}, publisher = {Research Institute of Forests and Rangelands}, issn = {1735-0913}, eissn = {2383-112X}, doi = {10.22092/ijwpr.2017.109576}, abstract = {Wood industries need abundant resources of wooden raw material and these industries could continue to productive activities with poplar consumption attitudes. Given the size and importance of poplar farming and its role in the economy of Kurdistan, study for evaluation of its value chain is essential. Since improving of the poplar value chain is a factor for the development of poplar farming given the current situation in Kurdistan providence value chain, in this research suitable value chains was identified for development. According to the study objectives, the effective criteria to prioritize research alternatives were identified through library studies and with the help of questionnaires were completed and confirmed, according to the experts. The experts were used to identify the interrelations between criteria. After completing the paired comparison questionnaire, weight of each criterion was measured and priorities were found by the ANP. Ultimately, the final results of alternatives ranking showed the most weight is related to the MDF chain with weight of 0.259. The next priorities were paper, straw and cellulose with respectively weights of 0.135, 0.134 and 0.115. The next priorities were furniture, particle board, plywood and matches, pallets, boxes, lumber and boards, with weights of 0.096, 0.077, 0.075, 0.073 and 0.019 respectively. Results of group decision-making using ANP showed that in the current situation with regard to the suitable market for MDF, proper future demand, appropriate market for processed products from MDF, condition of infrastructure in Kordestan province and feasibility of use of poplar wood in production of MDF, this industry is more important to develop in Kordestan province.}, keywords = {Poplar,Value chain,Kurdistan,Analytic network process}, title_fa = {اولویت‌بندی صنایع فرآوری چوب صنوبر در استان کردستان با هدف بهسازی زنجیره ارزش چوب صنوبر}, abstract_fa = {صنایع چوب به منابع فراوان ماده اولیه چوبی نیاز دارند و این صنایع با رویکرد مصرف چوب صنوبر، می‌توانند به فعالیت‌های تولیدی ادامه دهند. با توجه به وسعت و اهمیت صنوبرکاری و نقش آن در اقتصاد استان کردستان، مطالعه در زمینه بررسی زنجیره ارزش آن ضروری است. از آنجایی که بهبود زنجیره ارزش صنوبر عاملی برای توسعه زراعت آن است، در این پژوهش با توجه به شرایط موجود در زنجیره ارزش چوب صنوبردر استان کردستان، اولویت صنایع فرآوری قابل توسعه مشخص شد و با توجه به اهداف تحقیق معیارهای مؤثر بر اولویت‌بندی گزینه‌های تحقیق از طریق مطالعات کتابخانه‌ای شناسایی و با کمک پرسشنامه و طبق نظر متخصصین تکمیل و تایید شد. برای شناسایی روابط درونی میان معیارها از نظر متخصص‌ها استفاده شد. پس از تکمیل پرسشنامه مقایسه زوجی وزن هر یک از معیارها و اولویت‌ها به‌وسیله فرآیند تحلیل شبکه‌ای مشخص شد. نتایج نهایی حاصل از اولویت‌بندی گزینه‌ها نشان داد، بیشترین وزن مربوط به زنجیره ارزش تخته فیبر با دانسیته متوسط با مقدار 259/0 است. گزینه‌های بعدی دارای اولویت توسعه شامل تولید کاغذ، پوشال و سلولز بودند که به ترتیب دارای وزن‌های 135/0 و 134/0 و 115/0 بودند. پس از آن مبلمان، تخته خرده چوب، تخته لایه و کبریت، پالت و جعبه و الوار و تخته به ترتیب با وزن‌های 096/0، 077/0، 075/0، 073/0 و 019/0 قرار داشتند. نتایج تصمیم‌گیری گروهی به روش فرآیند تحلیل شبکه‌ای نشان داد، در شرایط کنونی با توجه به بازار مناسب تخته فیبر با دانسیته متوسط، شرایط آینده تقاضای آن، بازار مناسب محصولات فرآوری شده آن، شرایط زیرساخت‌ها در استان کردستان و با توجه به اینکه امکان استفاده از چوب صنوبر به عنوان ماده اولیه تولید تخته فیبر با دانسیته متوسط فراهم است، این صنعت، در استان کردستان، برای توسعه از اهمیت بیشتری برخوردار است.}, keywords_fa = {صنوبر,زنجیره ارزش,کردستان,فرآیند تحلیل شبکه‌ای}, url = {https://ijwpr.areeo.ac.ir/article_109576.html}, eprint = {https://ijwpr.areeo.ac.ir/article_109576_ca3e77c102d46a8a959f32bcea85e741.pdf} } @article { author = {Hemmasi, Amir Homan and kohantorabi, mostafa}, title = {Investigation of relationship between dynamic modulus of elasticity and static bending ‎properties in ‎particleboard plates}, journal = {Iranian Journal of Wood and Paper Science Research}, volume = {32}, number = {2}, pages = {193-204}, year = {2017}, publisher = {Research Institute of Forests and Rangelands}, issn = {1735-0913}, eissn = {2383-112X}, doi = {10.22092/ijwpr.2017.109577}, abstract = {In this study the relationship between dynamic modulus of elasticity from longitudinal ‎vibration ‎method with static modulus of elasticity and bending strength in two directions: the ‎Parallel ‎machine direction and machine direction have been investigated. For this purpose 4 ‎plates of ‎particleboard with dimensions 124× 90 ×1.6 cm (length× width× thickness) were ‎selected and free ‎longitudinal vibration test in PMD and MD were performed on each plates. ‎After that the primary ‎plates were cut to four plates with dimensions 62× 44 ×1.6 cm (length× ‎width× thickness) and ‎longitudinal vibration test in PMD and MD were performed on each ‎plates again. Finally each plates ‎were cut to the beams with dimensions 36× 1.6 ×1.6 cm and ‎longitudinal vibration test and and ‎static bending test were performed on them. The results show ‎that good correlation between ‎dynamic modulus of elasticity from longitudinal vibration test ‎and static modulus of elasticity and ‎bending strength (result of beams extracted from each ‎plates) in both size of plates in two size ‎‎(124× 90 ×1.6 and 62× 44 ×1.6 cm) and beams ‎extracted from each plates in two directions (PMD ‎and MD). In addition there was good ‎correlation between dynamic modulus of elasticity of ‎longitudinal vibration from two size plates ‎‎(124× 90 ×1.6 and 62× 44 ×1.6 cm). When the samples ‎smaller than primary plates, the ‎dynamic modulus of elasticity values were increased, that it due to ‎the diffusion of waves in ‎samples with larger dimensions. In general, according to results of this ‎research it can be ‎concluded that by applying the appropriate correction factors, longitudinal ‎vibration method an ‎efficiency method for calculation of dynamic and static modulus of elasticity ‎and estimate of ‎the modulus of rupture in plates in full sized.‎}, keywords = {Vibration,Plate,STATIC BENDING,Modulus of elasticity,Non-destructive}, title_fa = {بررسی رابطه بین مدول الاستیسیته دینامیک در صفحات تخته خرده چوب با مدول الاستیسیته استاتیک و ‏مقاومت خمشی}, abstract_fa = {در این تحقیق به بررسی رابطه بین مدول الاستیسیته دینامیک حاصل از ارتعاش طولی صفحات تخته خرده چوب با ‏مدول ‏الاستیسیته استاتیک و مقاومت خمشی در دو ‏جهت: خلاف جهت و جهت ماشین پرداخته شده است. بدین منظور ‏در ابتدا 4 ‏صفحه تخته خرده چوب با ابعاد 6/1×90×124 (طول×عرض×ضخامت) سانتی متر انتخاب ‏شدند و در دو ‏جهت خلاف جهت ‏ماشین و جهت ماشین مورد ارتعاش طولی قرار گرفتند. سپس از صفحات اولیه تعداد 4 صفحه با ‏ابعاد ‏6/1×44×62 ‏سانتی ‏متر انتخاب و ‏آزمون ارتعاش طولی در دو جهت خلاف جهت ماشین و جهت ماشین مجددا بر ‏روی صفحات صورت پذیرفت. ‏در نهایت صفحات به تیرهای با ابعاد ‏6/1×6/1×36 ‏سانتی متر ‏تبدیل شده و آزمون ‏ارتعاش طولی و خمش استاتیک بر روی ‏تیرها صورت گرفت. نتایج حاکی از همبستگی مطلوب بین نتایج حاصل از آزمون ‏ارتعاش طولی هر دو ابعاد ‏صفحات در دو ‏جهت ماشین و خلاف جهت ماشین و نتایج مدول الاستیسیته دینامیک و ‏استاتیک و همچنین مقاومت خمشی تیرهای مستخرج ‏شده از صفحات بود. ضمن ‏اینکه بین مدول الاستیسیته دینامیک ‏صفحات با ابعاد 6/1×90×124 و 6/1×44×62 سانتی متر ‏در دو جهت مورد آزمون همبستگی بسیار مطلوبی برقرار می ‏باشد. با کوچک ‏تر شدن ابعاد نمونه های آزمونی مقادیر مدول ‏الاستیسیته دینامیک افزایش یافت که این امر به دلیل ‏پراکندگی امواج در نمونه های با ابعاد بزرگتر می باشد. به طور کل با ‏توجه ‏به نتایج می توان اذعان داشت که با اعمال ‏ضرائب اصلاحی مناسب، روش ارتعاش طولی روشی کارا جهت محاسبه ‏مدول الاستیسیته و تخمین مدول گسیختگی ‏صفحات ‏تخته خرده چوب در ابعاد کامل می باشد.‏}, keywords_fa = {ارتعاش,صفحه,خمش استاتیک,مدول الاستیسیته,غیرمخرب}, url = {https://ijwpr.areeo.ac.ir/article_109577.html}, eprint = {https://ijwpr.areeo.ac.ir/article_109577_238db8f2c3f846d6c5e810f8a1e82784.pdf} } @article { author = {Hasani Khorshidi, Fatemeh and Emadi, Mehdi}, title = {Studying effect of accelerated aging on adhesion resistance of half polyester and polyurethane transparent coatings applied on maple and pine species}, journal = {Iranian Journal of Wood and Paper Science Research}, volume = {32}, number = {2}, pages = {205-214}, year = {2017}, publisher = {Research Institute of Forests and Rangelands}, issn = {1735-0913}, eissn = {2383-112X}, doi = {10.22092/ijwpr.2017.109580}, abstract = {In this study, effect of accelerated aging on adhesion strength of half-polyester and polyurethane transparent coatings were evaluated in maple and pine species. For this purpose, dried specimens with 12×110×550 millimeters were used. Sealer as substrate, and half-polyester and binary polyurethane as coatings were applied on wood. Coatings were implemented thereby film applicator and gun methods, and accelerated aging test of wood specimens was carried out according to ASTM D1037. Results indicated that maximum value of adhesion strength is belong to binary polyurethane in maple applied by film applicator and minimum for half-polyester in pine applied by gun method, in opposite. Due to thin film, velocity variations in gun method by painter person, and consequent rapid evaporation of thinner, adhesion decreased in comparison with film applicator method. Also it's found that accelerated aging diminished adhesion strength of coatings in both maple and pine species. It can be concluded during the accelerated aging test, the steam causes moisture absorption and swelling of the fibers near the surface and thus reduce the resistance of the coating adhesion.Long-term effect of humidity and aging makes Ecowool quickly lose their stickiness.And the effect of floating in the water samples, lignin degradation products in the process of steaming and freezing and heating washed by water And cause the loosening of the cellulosic fibers in the wood, resulting in wood adhesive strength is significantly reduced due to the accelerated aging test.}, keywords = {accelerated aging,MAPLE,pine,Adhesion strength,half-polyester,Polyurethane}, title_fa = {بررسی اثر کهنگی تسریع شده بر مقاومت چسبندگی شفاف‌پوشه های نیم پلی‌استر و پلی‌اورتان اعمال شده در گونه های افرا و کاج}, abstract_fa = {در این پژوهش تاثیر کهنگی تسریع شده بر مقاومت چسبندگی شفاف ‌پوشه های نیم پلی استر و پلی‌اورتان در گونه‌های افرا(acer)با PH6از منطقه ی شمال کشور و سوزنی برگ کاج(pinus) با PH 5.5 از چوب های وارداتی کشور روسیه مورد مطالعه و ارزیابی قرار گرفته است. بدین منظور، از نمونه های با ابعاد 12×110×550 میلی‌متری خشک شده استفاده شد. همچنین از سیلر به عنوان زیرآیند پوشش‌ها، و نیم پلی استر و پلی‌اورتان دوجزئی نیز جهتِ پوشش‌دهی نمونه‌های چوب استفاده شد. پوشش دهی به روش پیستوله انجام گرفته و تاثیر کهنگی تسریع شده بر نمونه های چوب مطابق با ASTM D1037 مورد آزمون قرار گرفت. نتایج نشان داد که بیشترین مقدار مقاومت چسبندگی مربوط به شفاف ‌پوشه پلی‌اورتان دوجزئی و در گونه‌ی افرا و کمترین مقدار در گونه کاج و شفاف پوشه نیم پلی‌استر می باشد. مشاهده شد که کهنگی تسریع‌شده باعث کاهش مقاومت چسبندگی شفاف ‌پوشه‌ها در گونه‌های چوبی افرا و کاج می‌شود.می توان نتیجه گرفت درطی آزمون کهنگی تسریع شده، مرحله بخاردهی باعث جذب رطوبت نمونه ها و ایجاد واکشیدگی در الیاف نزدیک سطوح و در نتیجه کاهش مقاومت چسبندگی پوشش می‌شود. تاثیر بلندمدت رطوبت و کهنگی باعث می شود که پوشش های سلولزی به سرعت چسبندگی شان را از دست بدهند.و در اثر مرحله شناوری سازی نمونه ها در آب، محصولات تخریب شده لیگنینی در مراحل بخار دهی و فریز و گرما دهی توسط آب شسته شده و موجب سست شدن الیاف سلولزی در سطح چوب می شود، در نتیجه مقاومت چسبندگی چوب به میزان قابل توجهی در اثر آزمون کهنگی تسریع شده کاهش می یابد.}, keywords_fa = {کهنگی تسریع شده,افرا,کاج,مقاومت چسبندگی,نیم پلی استر,پلی اورتان}, url = {https://ijwpr.areeo.ac.ir/article_109580.html}, eprint = {https://ijwpr.areeo.ac.ir/article_109580_4efba94301700bea2b9d1885a77640da.pdf} } @article { author = {Rodi, Hamid reza and Jalali Torshizi, Hossein and Rasooly Garmaroudy, Esmaeil}, title = {Comparison of filler type performance on paper properties in the presence of cationic rosin sizing agent}, journal = {Iranian Journal of Wood and Paper Science Research}, volume = {32}, number = {2}, pages = {215-226}, year = {2017}, publisher = {Research Institute of Forests and Rangelands}, issn = {1735-0913}, eissn = {2383-112X}, doi = {10.22092/ijwpr.2017.109578}, abstract = {The aim of this study was to investigate the effect of using different fillers in the presence of cationic rosin sizing agent on the properties of pulp and paper made from CMP fibers. For this purpose, cationic rosin internal sizing agent at the levels of 0, 0.5, 1 and 1.5 % based on oven dry fibers, and fillers including grounded carbonate calcium (GCC), precipitated carbonate calcium (PCC), Talc and Zeolite in 25 % level based on oven dry paper accompanied with cationic polyacrylamide retention agent at the constant level of 0.3 % based on oven dry fibers were added to the CMP pulp suspension according to the TAPPI standard. In order to examine the effect of different fillers in the presence of cationic rosin, handsheets with basis weight of about 60±3 g/m2 were prepared from each experiment. Then, various pulp and paper characteristics were measured. Statistical analysis of the results revealed that type of filler has dissimilar behavior on the pulp and paper properties in the presence of cationic rosin. Drainage time of pulp suspension was lower when adding Zeolite and GCC fillers. Talc and PCC decreased more the paper strengths properties. Ultimately optical properties of papers improved more when Talc and PCC were added to the CMP pulp. Consequently, with respect to the priority of brightness and opacity for the copy and print papers made from CMP fibers, addition of Talc and PCC in the presence of cationic rosin sizing agent may be meet more the requirements compare to Zeolite and GCC fillers.}, keywords = {Fillers,cationic rosin,Paper properties,carbonate calcium,Talc,Zeolite}, title_fa = {مقایسه عملکرد نوع پرکننده‌ بر ویژگی‌های کاغذ در حضور عامل آهاردهی روزین کاتیونی}, abstract_fa = {این پژوهش با هدف بررسی تأثیر استفاده از پرکننده‌های مختلف در حضور عامل آهاردهی روزین کاتیونی بر ویژگی‌های مختلف کاغذ تهیه‌شده از الیاف خمیرکاغذ CMP انجام شده‌است. از این رو عامل آهاردهی داخلی روزین کاتیونی در سطوح 0، 5/0، 1 و 5/1 درصد براساس وزن خشک الیاف و پرکننده‌های کربنات کلسیم آسیابی (GCC)، کربنات کلسیم رسوبی (PCC)، تالک (Talc) و میکروزئولیت (Microzeolite) در سطح 25 درصد بر اساس وزن خشک کاغذ به‌همراه عامل کمک‌نگهدارنده پلی‌اکریل آمید کاتیونی در سطح ثابت 3/0 درصد براساس وزن خشک الیاف، در ترکیب سوسپانسیون خمیرکاغذ CMP مطابق استاندارد TAPPI اعمال شد. به منظور بررسی اثر پرکننده‌های مختلف در حضور عامل آهاردهی، از هر نوع تیمار کاغذهای دست‌ساز با گراماژ 3±60 گرم بر مترمربع تهیه‌شد. سپس خواص مختلف کاغذ تهیه‌شده اندازه‌گیری شد. تحلیل آماری نتایج نشان داد که نوع پرکننده در کاغذ بر ویژگی‌های مختلف کاغذ رفتار متفاوتی در حضور روزین کاتیونی دارد. سوسپانسیون خمیرکاغذ به‌هنگام افزودن پرکننده‌های زئولیت و GCC زمان آبگیری کمتری نشان‌داد. پرکننده‌های تالک و PCC مقاومت‌های کاغذ را بیشتر کاهش دادند. و در نهایت ویژگی‌های نوری کاغذ زمانی بهبود یافت که تالک، PCC به خمیرکاغذ CMP اضافه شد. در نتیجه با توجه به اهمیت خواص روشنی و ماتی برای کاغذ چاپ و تحریری که از خمیرکاغذ CMP تهیه می‌شوند، افزودن تالک و PCCدر حضور عامل آهار روزین کاتیونی می‌تواند نسبت به پرکننده‌های زئولیت و GCC نیازها را بیشتر برآورده سازد.}, keywords_fa = {پرکننده,روزین کاتیونی,ویژگی‌های کاغذ,کربنات کلسیم,تالک,میکروزئولیت}, url = {https://ijwpr.areeo.ac.ir/article_109578.html}, eprint = {https://ijwpr.areeo.ac.ir/article_109578_3889db81c9fdd8c71a918d07aa83aef1.pdf} } @article { author = {Jahanshahlou, Sobhan and Khosravani, Amir and Rahmaninia, Mehdi}, title = {Comparing the Effect of Silica Sol and Bentonite Nanoparticles on the Performance of Cationic Starch for Drainability, Retention and Strength Properties of Recycled Paper}, journal = {Iranian Journal of Wood and Paper Science Research}, volume = {32}, number = {2}, pages = {227-237}, year = {2017}, publisher = {Research Institute of Forests and Rangelands}, issn = {1735-0913}, eissn = {2383-112X}, doi = {10.22092/ijwpr.2017.109583}, abstract = {Production of test liner and fluting from old corrugated containers, is one of the most common paper recycling processes in Iran. This type of papers, have high basis weight and also contain significant fine fibrous and non-fibrous materials; hence, the drainage and in addition, the retention of fine materials, are the obstacles these paper mills may encounter. In these cases, usually application of drainage/retention aids, such as nanoparticle systems can be of much help. In this due, colloidal silica and bentonite are the two of the most commonly used nano-particles with polyelectrolytes in papermaking wet-end. Therefore, in this research, the effect of bentonite and silica sol nano-particles on the performance of cationic starch was compared in terms of drainability, retention and strength properties of paperboard from recycled old corrugated containers. The analysis of the particle size for these two nanoparticles showed that although the thickness of bentonite platelets (maximum 22 nm) was less than nanosilica dimensions (less than 50 nm), the effect of bentonite-cationic starch was not significant in terms of retention, against the nanosilica. Regarding the drainability, following dosing of both silica and bentonite, the parameter much improved (up to 186% in the case of nanosilica). On the other hand, application of cationic starch containing systems in paper handsheets resulted in improvement in tensile and tear indices, however, these properties decreased following addition of nano-particles. Also, internal bonding (Scott- type) incredibly increased (up to 354%) by application of cationic starch and nanosilica. At last, generally in the case of OCC furnish, the nanosilica-cationic starch system had a better performance in terms of drainability, retention of fine materials and fiber fines and also strength properties, rather than cationic starch-bentonite.}, keywords = {nanosilica,Nanobentonite,cationic starch,Old corrugated container,Drainability}, title_fa = {مقایسه اثر نانوذرات سیلیکاسل و بنتونیت بر عملکرد نشاسته کاتیونی به لحاظ قابلیت آبگیری، ماندگاری و ویژگی های مقاومتی کاغذ بازیافتی}, abstract_fa = {تولید انواع تست لاینر و فلوتینگ از کارتن‌های کنگره‌ای کهنه، یکی از رایج‌ترین فرآیندهای بازیافت کاغذ در ایران می‌باشد. این نوع کاغذ، دارای وزن پایه زیاد و حاوی مقادیر قابل توجهی قطعات ریز لیفی و غیرلیفی است و لذا معمولا آبگیری از این نوع مقوا و نیز ماندگاری ذرات ریز، از معضلات اینگونه کارخانجات به‌حساب می‌آید. از این‌رو در چنین مواردی استفاده از مواد کمک آبگیری/ماندگاری، مانند سیستم‌های برپایه نانوذرات می‌تواند راهگشا باشد. درهمین ارتباط از رایجترین و پرمصرف‌ترین انواع نانوذرات مورد استفاده در صنعت کاغذ، دو نوع نانوذره سیلیکای‌ کلوییدی و بنتونیت هستند که به همراه پلی الکترولیت‌های کاتیونی در پایانه تر کاغذسازی قابل استفاده می‌باشند. بنابراین در این مطالعه، اثر نانوذرات بنتونیت و سیلیکاسل، بطور مقایسه‌ای، بر عملکرد نشاسته‌کاتیونی به لحاظ قابلیت آبگیری، ماندگاری و ویژگی‌های مقاومتی مقوای حاصل از بازیافت کارتن‌های کنگره-ای کهنه مورد بررسی قرارگرفت. نتایج بررسی ابعاد این دو نوع نانوذره نشان داد، هرچند میانگین ضخامت ورقه‌های بنتونیت (حداکثر 22 نانومتر) از میانگین ابعاد نانوذره کروی سیلیکای کلوییدی (کمتر از 50 نانومتر) کوچکتر بوده است اما به لحاظ شاخص ماندگاری، برخلاف نانوسیلیکا، اثر نانوبنتونیت- نشاسته کاتیونی معنی‌دار نبود. در خصوص قابلیت آبگیری، با افزودن هر دو نوع نانوذره نانوسیلیکا و نانوبنتونیت، این ویژگی بهبود قابل ملاحظه‌ای ( حتی تا مقدار 186% در خصوص نانوسیلیکا) داشته است. از سوی دیگر، استفاده از نشاسته کاتیونی در کاغذ دست‌ساز، سبب بهبود شاخص‌‌های مقاومت به کشش و پاره‌شدن گردید، در حالی‌که این ویژگی‌ها با افزودن نانوذرات، کاهش یافت. همچنین مقاومت پیوند درونی کاغذ، با افزودن نشاسته کاتیونی و نانوسیلیکا افزایش فوق‌العاده‌ای (تا 354%) نشان داد. در نهایت به طور کلی، در خمیر کاغذ OCC، سیستم نشاسته کاتیونی- نانوسیلیکا به لحاظ قابلیت آبگیری، ماندگاری ذرات ریز و همچنین ویژگی‌های مقاومتی، عملکرد بهتری نسبت به سیستم نشاسته کاتیونی- نانوبنتونیت داشته است.}, keywords_fa = {نانوسیلیکا,نانوبنتونیت,نشاسته کاتیونی,کارتن کنگره‌ای کهنه,قابلیت آبگیری}, url = {https://ijwpr.areeo.ac.ir/article_109583.html}, eprint = {https://ijwpr.areeo.ac.ir/article_109583_5b86f1ec2acb67963808a12711e16df8.pdf} } @article { author = {Naijian, Fatemeh and Resalati, Hossein and Rodi, Hamid reza and Jalali-Torshizi, Hossein and Pirmoradian, Kamal}, title = {Effect of alum-cationic rosin consumption level on the properties of papers made from recycled white sheets trimmings}, journal = {Iranian Journal of Wood and Paper Science Research}, volume = {32}, number = {2}, pages = {238-250}, year = {2017}, publisher = {Research Institute of Forests and Rangelands}, issn = {1735-0913}, eissn = {2383-112X}, doi = {10.22092/ijwpr.2017.109581}, abstract = {Nowadays, recycled fibers are the main fiber source for manufacturing packaging papers. Sizing of such papers, based on the type of application, is of great importance. In this research, the effect of alum-cationic rosin consumption amount in pH of about 6.5 on the properties of papers made from white sheets trimmings was examined. In order to optimize consumption extent, pulp suspension sizing with alum in six level of 0, 4, 5, 7, 8, and 10 %, and rosin with the ratio of 50 % of alum based on oven dry (OD) pulp was done according to the TAPPI standard methods. Then by preparation of handsheets with basis weight of about 65±5 g/m2, their Cobb test (45 second), structural and strength characteristics were investigated. Statistical analysis of the results have shown that alum and rosin consumption amount of about 7 and 3.5 % based on OD pulp is the best suitable level for internal sizing of white sheets trimmings fibers. In these alum-rosin level, Cobb value of papers decreased from 120±11.6 g/m2 the lowest value of about 64±9.7 g/m2. Contact angle of water droplet with the paper surface increased from 24.81º to 96.53º. Paper tensile index decreased up to 125±9.7 N.m/g by such sizing level and again increased with increasing alum-rosin level. Seemingly, such phenomena can be attributed to the alum role in charge neutralizing, cellulosic fines retention and improving bonding-ability of paper network. Meaningful decrease of paper surface roughness from 10.34±0.54 µm in control sample to 8.23±1.37 µm in sized papers in optimized level confirmed this assumption.}, keywords = {Rosin,alum,Paper properties,recycled fibers,white sheets trimmings,Contact angle}, title_fa = {تأثیر سطح مصرف آلوم – روزین کاتیونی بر ویژگی‌های کاغذ تهیه‌شده از بازیافت کناره‌بری ورقه‌های سفید}, abstract_fa = {امروزه الیاف بازیافتی منبع فیبری عمده برای تهیه کاغذهای بسته‌بندی می‌باشد. بسته به نوع کاربرد، آهاردهی این نوع کاغذها از اهمیت بسیار بالایی برخوردار است. در این تحقیق، اثر میزان مصرف آلوم-روزین کاتیونی در pH حدود 5/6 بر ویژگی‌های کاغذهای تهیه‌شده از کناره‌بری ورقه‌های سفید بررسی شده‌است. جهت بهینه‌سازی میزان مصرف، آهاردهی سوسپانسیون خمیرکاغذ با آلوم در 6 سطح 0، 4، 5، 7، 8 و 10 درصد و روزین با نسبت 50 درصد آلوم در هر سطح برمبنای وزن خشک خمیرکاغذ مطابق استاندارد TAPPI اعمال شد. سپس با تهیه کاغذهای با گراماژ g/m2 5±65، ویژگی‌های جذب آب (45 ثانیه)، ساختاری و مقاومتی آنها مورد ارزیابی قرار گرفت. تحلیل آماری نتایج نشان داد که میزان مصرف آلوم و روزین به‌ترتیب 7 و 5/3 درصد بر مبنای خشک خمیرکاغذ مناسب‌ترین سطح بکارگیری این ترکیب برای آهاردهی داخلی الیاف ورقه‌های کناره‌بری‌ سفید می‌باشد. در این سطح آلوم-روزین، جذب آب کاغذها از g/m2 6/11±120 به کمترین مقدار و تا حدود g/m2 7/9±64 کاهش یافت. زاویه تماس قطره آب با سطح کاغذ از 81/24 درجه به 53/96 درجه افزایش یافت. شاخص کششی کاغذ تا این سطح آهاردهی تا حدود N.m/g 7/9±125 کاهش و سپس با افزایش سطح آلوم-روزین این مقاومت افزایش یافت. بنظر می‌رسد این پدیده به‌علت نقش آلوم در خنثی‌سازی بار آنیونی، ماندگاری نرمه‌های سلولزی و توسعه قابلیت پیوندیابی شبکه کاغذ باشد. کاهش معنی‌دار زبری سطح کاغذ از µm 54/0±34/10 در نمونه شاهد به µm 37/1±8/23 در کاغذ آهار شده در سطح بهینه تأییدکننده این فرضیه می-باشد.}, keywords_fa = {روزین,آلوم,ویژگی‌های کاغذ,الیاف بازیافتی,کناره‌بری ورقه‌های سفید,زاویه تماس}, url = {https://ijwpr.areeo.ac.ir/article_109581.html}, eprint = {https://ijwpr.areeo.ac.ir/article_109581_1134da8150dca9c00b66723f9093bc63.pdf} } @article { author = {Kargarfard, Abolfazl}, title = {Investigation on the Effect of Resin Gradient Consumption on Particleboard Properties Made Using Rose Flower Stalks Residues}, journal = {Iranian Journal of Wood and Paper Science Research}, volume = {32}, number = {2}, pages = {251-260}, year = {2017}, publisher = {Research Institute of Forests and Rangelands}, issn = {1735-0913}, eissn = {2383-112X}, doi = {10.22092/ijwpr.2017.106283}, abstract = {Investigation on the Effect of Resin Gradient Consumption on Particleboard Properties Made Using Rose Flower Stalks Residues Abolfazl Kargarfard *Associate Prof., Wood and Paper Science and technology Research Division, Research Institute of Forests and rangeland, Tehran, Iran, kargarfard@rifr-ac.irAbstractThe potential of rose flower stalks for the production of particleboard was investigated. Three resin dosage gradients of 0, 2 and 4% (10% core: 10% surface; 9%core:11% surface and 8% core:12% surface) and three press times (3, 4 and 5 minutes) were selected as the variables and boards were produced. Then the mechanical and physical properties of the boards were measured and statistically analyzed. The results of modulus of rupture (MOR), modulus of elasticity (MOE) and internal bonding (IB) measurements showed that as the resin dosage gradient increases, these properties improved and boards produced using either 2 or 4% resin dosage gradients generated the highest values. The effect of resin dosage gradient on these properties was statistically significant. As the resin dosage gradient increases, both thickness swelling after 2 and 24 hours immersion in water was improved. The effect of press time on thickness swelling after 2 and 24 hours immersion in water was also statistically significant and these properties were improved when 5 minutes press time was used The results indicate that if 2 or 4% resin dosage gradients and either 4 or 5 minutes press time is applied for the manufacturing of particleboards using rose flower stalks residues, the specification of the boards will meet the EN specification.Keywords: Particleboard, Rose flower stalks, Resin dosage gradient, Mechanical Properties, Physical Properties}, keywords = {Keywords: Particleboard,Rose flower stalks,Resin dosage gradient,MECHANICAL PROPERTIES,physical properties}, title_fa = {بررسی اثر اختلاف مصرف چسب بین لایه سطحی و میانی بر ویژگیهای تخته خرده چوب ساخته شده از پسماند هرس بوته گل محمدی}, abstract_fa = {چکیدهدر این تحقیق، امکان استفاده از ساقه گل محمدی در تولید تخته خرده چوب مورد بررسی قرار کرفت. لذا با استفاده از 3 گرادیان مصرف چسب صفر، 2 و 4 درصد بین لایه سطحی و میانی کیک خرده چوب (10 - 10؛ 11 - 9 و 12 - 8 درصد)؛ و 3 زمان پرس 3؛ 4 و 5 دقیقه و کاربرد ساقه گل محمدی به عنوان ماده اولیه چوبی اقدام به ساخت تخته های آزمایشگاهی گردید و خواص فیزیکی و مکانیکی آنها اندازه گیری و مورد تجزیه و تحلیل قرار گرفت. نتایج نشان داد که بیشترین مقاومت خمشی (MOR) و مدول الاستیسیته (MOE) تخته ها در گرادیان مصرف چسب 2 درصد حاصل شده است. همچنین با افزایش زمان پرس، این ویژگیها با کاهش معنی داری از نظر آماری روبرو شده اند. در حالی که تخته های ساخته شده با زمان پرس 4 دقیقه از چسبندگی داخلی بالاتری برخوردار بودند. همچنین گرادیان مصرف چسب اثر معنی داری بر واکشیدگی ضخامت 2 ساعت داشت و کمترین واکشیدگی ضخامت 2 ساعت تخته ها در گرادیان مصرف چسب 2 درصد مشاهده شد. علاوه بر این، زمان پرس نیز اثر معنی داری بر این ویژگی تخته ها داشت و حداقل واکشیدگی ضخامت 2 و 24 ساعت در شرایط استفاده از زمان پرس 3 دقیقه حاصل گردید. نتایج این تحقیق نشان داد که در صورت استفاده از گرادیان مصرف چسب در حد 2 درصد بین لایه سطحی و میانی کیک خرده چوب و زمان پرس 3 دقیقه، می توان از ساقه گل محمدی به عنوان یک ماده لیگنوسلولزی مناسب برای تولید تخته خرده چوب با ویژگیهای مکانیکی بالاتر از استاندارد EN اروپا استفاده نمود.}, keywords_fa = {واژه های کلیدی: تخته خرده چوب,ساقه بوته گل محمدی,گرادیان مصرف چسب,خواص مکانیکی,خواص فیزیکی}, url = {https://ijwpr.areeo.ac.ir/article_106283.html}, eprint = {https://ijwpr.areeo.ac.ir/article_106283_77f869a8649812ff5d35ef8d93fdcd29.pdf} } @article { author = {abdolalizadeh, Mahboob and Azadi, Mehrnaz and Mohammadi achzchluei, Mohsen}, title = {Study of side effects of Thiophanate-methyl fungicide on aesthetic and structural properties of ‎paper}, journal = {Iranian Journal of Wood and Paper Science Research}, volume = {32}, number = {2}, pages = {261-274}, year = {2017}, publisher = {Research Institute of Forests and Rangelands}, issn = {1735-0913}, eissn = {2383-112X}, doi = {10.22092/ijwpr.2017.113142}, abstract = {‎ The most of the fungicide‏ ‏that are used to prevent or stop the biological destruction of the historical papers have been used ‎at the first time in domains of science and industrial So thiophanate methyl which is most useful in agriculture, have been ‎tested in repairing and protection of papers and it’s one of the most useful materials in agriculture antifungals.The main ‎aim of this research was assessment of aesthetic and structural effects on paper after treatment by Thiophanate-methyl ‎compound. Experimental method (laboratory experience) and library study wre applied in this research. ATR-FTIR spectra ‎showed that spray of Thiophanate-methyl on paper did not produce any degradation effect. The compound had not ‎changed aesthetical properties and pH values. Tensile strength of paper did not reduce due to the treatment. This indicates ‎nondestructive effects of Thiophanate-methyl on paper which signifies its great capability for application in conservation ‎and restoration of paper.‎}, keywords = {PAPER,Fungicide,side effect,structural change,conservation and restoration ‎}, title_fa = {بررسی تأثیرات قارچ‌کش تیوفانات متیل بر ویژگی‌های بصری و ساختاری کاغذ}, abstract_fa = {‏اکثر روش‌های قارچ زدایی که برای پیشگیری یا توقف زوال بیولوژیکی کاغذهای تاریخی استفاده می‌شوند، ابتدا در دیگر زمینه‌های ‏علمی و صنعتی مورد استفاده قرار گرفته‌اند. از این رو همواره علوم دیگر نقش مهمی در رفع مشکلات موجود در آفت‌زدایی آثار، علی-‏الخصوص آثار کاغذی داشته است. به همین دلیل قارچ کش‌ تیوفانات متیل که از پر کاربردترین و مهم‌ترین مواد در کشاورزی است و ‏بر طیف وسیعی از آفات بیولوژیکی مورداستفاده قرار می‌گیرد، جهت استفاده‌ی آن در حفاظت و مرمت آثار کاغذی مورد ارزیابی قرار ‏گرفت. بر این اساس هدف اصلی این پژوهش، بررسی تأثیرات ساختاری و بصری کاغذ بعد از درمان با ماده‌ی تیوفانات متیل است. ‏روش تجربی‎ ‎‏(آزمایشگاهی) و مطالعه کتابخانه‌ای در این پژوهش به کار گرفته شده است. بررسی طیف‌های ‏ATR-FTIR‏ بدست آمده ‏از نمونه‌ها، نشان داد که بکارگیری تیوفانات متیل به روش اسپری بر کاغذ فیلتر، باعث تخریب ساختار کاغذ نمی‌شود. این ماده بر ‏ویژگی‌های بصری کاغذ تغییر شدیدی نداشته و بر ‏pH‏ کاغذها در فرایند مطالعات تأثیر جدی ایجاد نکرد. مقاومت کششی نیز در ‏کاغذهای تیمار شده کاهشی را نشان نداد. این امر نشان دهنده عدم تاثیر تخریبی تیوفانات متیل بر کاغذ است که گویای قابلیت‌های ‏آن جهت استفاده در حفاظت کاغذ است.‏}, keywords_fa = {کاغذ,قارچ‌کش,تیوفانات متیل,تاثیر جانبی,تغییرات ساختاری,حفاظت و مرمت}, url = {https://ijwpr.areeo.ac.ir/article_113142.html}, eprint = {https://ijwpr.areeo.ac.ir/article_113142_172f79c98a3be32b125ca8dbcbefba22.pdf} } @article { author = {Vaysi, Ramin}, title = {A Study on the Possibility of Identification and Comparison of Metallic Ions and Chemical Components in Wood and Bark of Oak by Atomic Adsorption and GC-MS Methods}, journal = {Iranian Journal of Wood and Paper Science Research}, volume = {32}, number = {2}, pages = {275-286}, year = {2017}, publisher = {Research Institute of Forests and Rangelands}, issn = {1735-0913}, eissn = {2383-112X}, doi = {10.22092/ijwpr.2017.109582}, abstract = {The aim of study was accomplished on identification and comparison of chemical compounds in wood and bark of oak. For this purpose, the samples were chosen randomly from oak in Nowshahr forest region. Then, flour and ash were provided from heart wood, sap wood and bark of oak by TAPPI standards. For measured metallic ions, first the mineral compound of ash dissolved by 65% nitric acid and for it's identified by atomic adsorption method. The results showed that Fe, Zn and Cu ions in wood of oak were more than its bark and its Mn ion was lower. Then extractives were separated from wood flour by acetone and extractives residue transferred to glassy vial and was added BSTFA reactor to it. After samples prepared, its were injected by GC/MS for analyze. Identification of compounds was done by retention time of each compound, calculation of quartz index and Adams table. The result of GC-MS showed that there are 10, 42 and10 compounds in heart wood, sap wood and bark of oak, respectively. Comparison of chromatograms showed that Decan, Dodecan, Tetradecane and Bis(2-ethylhexyl)phthalate were exists as 4 common components in bark, sap wood and heart wood of oak and Silicic acid and 1,2-Benzenedicarboxylic acid were exists as 2 common components in bark and sap wood of oak. These compounds can very important in durability and consumption its.}, keywords = {Oak,Atomic Adsorption,Metallic Ions,Mass spectrometry,Gas chromatography,Organic compounds}, title_fa = {بررسی امکان شناسایی و مقایسه یون های فلزی و ترکیبات آلی موجود در چوب و پوست بلوط بلند مازو با استفاده ازفنون جذب اتمی، کروماتوگرافی گازی و طیف سنجی جرمی}, abstract_fa = {این تحقیق با هدف شناسایی و مقایسه یون های فلزی و ترکیبات آلی موجود در چوب و پوست بلوط بلند مازو انجام شد. به همین منظور نمونه های آزمونی از گونه بلوط بلند مازوی منطقه جنگل‌داری نوشهر به صورت تصادفی انتخاب گردید. سپس طبق آزمون های استاندارد TAPPI از درون چوب، برون چوب و پوست بلوط بلند مازو آرد چوب و خاکستر تهیه شد. برای تعیین یون های فلزی، ابتدا با کمک اسید نیتریک 65 درصد، مواد محلول موجود در خاکستر نمونه ها جداسازی و برای شناسایی از دستگاه جذب اتمی استفاده گردید. نتایج نشان داد که چوب بلوط نسبت به پوست آن دارای میزان جذب یون های آهن، روی و مس بیشتر و منگنز کمترمی باشد. سپس مواد استخراجی توسط حلال استن از آرد چوب جدا سازی گردید و باقیمانده مواد استخراجی به داخل یک ویال شیشه ای منتقل و به آن واکنشگر BSTFA اضافه شد. نمونه ها بعد از آماده سازی، به دستگاه GC-MSتزریق شدند. برای شناسایی ترکیبات نیز از دیاگرام زمان بازداری، محاسبه ضریب کواتز و جدول آدامز استفاده گردید. نتایج حاصل از GC-MS نشان داد که در درون چوب، برون چوب و پوست بلوط ‌بلند مازو بترتیب 10، 42 و 10 ترکیب شناسائی گردید. مقایسه کروماتوگرام ها نیز نشان داد که 4 ترکیب دکان، دودکان، تترادکان و بیس(2-اتیل هگزیل) فتالات در پوست، برون چوب و درون چوب بلوط و همچنین ترکیبات سالیسیک اسید و1و2-بنزن دی کربوکسیلیک اسید در برون چوب و پوست بلوط بلند مازو به صورت مشترک وجود دارد. این ترکیبات می توانند اهمیت زیادی در مصارف و دوام چوب بلوط داشته باشند.}, keywords_fa = {بلوط,یون فلزی,جذب اتمی,طیف سنجی جرمی,کروماتوگرافی گازی,ترکیبات آلی}, url = {https://ijwpr.areeo.ac.ir/article_109582.html}, eprint = {https://ijwpr.areeo.ac.ir/article_109582_c005cf41d00acb09e895e8e61799abd7.pdf} } @article { author = {Khodaparast, Sina and Jahan - Latibari, Ahmad and Rohnia, Mehran}, title = {The influence of compounding process on the properties of polypropylene-cellulosic fiber nanocomposite containing nanoclay particles.}, journal = {Iranian Journal of Wood and Paper Science Research}, volume = {32}, number = {2}, pages = {287-299}, year = {2017}, publisher = {Research Institute of Forests and Rangelands}, issn = {1735-0913}, eissn = {2383-112X}, doi = {10.22092/ijwpr.2017.109585}, abstract = {The effect of compounding process applying two methods of one and two step mixing on the properties of nanocomposite is investigated. Nanocomposites were produced using polypropylene, cellulosic fibers, MAPP and nanolay as reinforcement. 1.5 and 3% MAPP and 0,2, and 4% nanoclay were used as the variable factor and 20% fibers was used. Melt flow index was measured on compounds produced using one or two steps mixing. Either compounds were mixed with fibers and MAPP and then the test specimens were made and tested according to ASTM test procedures. The results revealed that the two steps mixing increased the mechanical properties. The melt flow index of one step mixing was lower and the melt flow index of initial mixing of polypropylene with nanoclay was very high and it was reduced after compounding with fibers and MAPP. The results revealed that at higher dosages of the nanoclay tensile and bending modulus of the composite increased and tensile strength and modulus of rupture decreased.}, keywords = {melt flow index,compounding,one step,two steps,MAPP. nanoclay}, title_fa = {تاثیر فرایند اختلاط مواد بر ویژگی های مقاومتی چندسازه الیاف سلولزی – پلی پروپیلن حاوی نانورس}, abstract_fa = {در این تحقیق تاثیر فرایند اختلاط به دو روش یک مرحله ای و دو مرحله ای بر ویژگی های ترکیب بدست آمده انجام گرفت. از پلی پروپیلن به عنوان ماده زمینه ای، الیاف سلولزی تقویت کننده، MAPP جفت کننده و نانورس پر کننده استفاده شده است. متغیرها شامل MAPP 5/1 و 3 درصد و نانورس 0 و 2 و 4 درصدبه عنوان متغیر و الیاف سلولزی به میزان 20% به طور ثابت انتخاب شده است. شاخص جریان مذاب اختلاط یک مرحله ای ( تمامی مواد با هم مخلوط و ترکیب شدند) و دو مرحله ای( ابتدا پلی پروپیلن با نانورس مخلوط شده و سپس ماده بدست آمده با الیاف و MAPP ترکیب شده اندازه گیری شده است. نمونه های آزمونی اندازه گیری مقاومت به کشش و خمش و ضربه فاقدار طبق آیین نامه، ASTM تهیه و مقاومت ها اندازه گیری شدند. در این تحقیق مشخص گردید روش دو مرحله ای بر ویژگی های مقاومتی تاثیر دارد و باعث افزایش خواص مکانیکی می شود.شاخص جریان مذاب در یک مرحله ای بسیار کم و در دو مرحله ای پس از مرحله اول بسیار زیاد و پس از مرحله دوم کم می باشد.نتایج نشان می دهد با افزایش مقدار نانورس مدول کشی و خمشی چندسازهالیاف سلولزی پلی پروپیلن افزایش و با افزایش مقدار نانورس مقاومت کششی و خمشی چندسازه الیاف سلولزی پلی پروپیلن افزایش داشته است.}, keywords_fa = {شاخص جریان مذاب,روش اختلاط,یک مرحله ای,دو مرحله ای,MAPP,نانورس}, url = {https://ijwpr.areeo.ac.ir/article_109585.html}, eprint = {https://ijwpr.areeo.ac.ir/article_109585_20affb766b98cc21c29ee0d6ec1ff44c.pdf} } @article { author = {Haghighi Poshtiri, Azar and Jonoobi, Mehdi and Karimi, Ali Naghi}, title = {Preparation of Cellulose Nanocrystals from α-Cellulose and Optimization of its Isolation Conditions}, journal = {Iranian Journal of Wood and Paper Science Research}, volume = {32}, number = {2}, pages = {300-310}, year = {2017}, publisher = {Research Institute of Forests and Rangelands}, issn = {1735-0913}, eissn = {2383-112X}, doi = {10.22092/ijwpr.2017.109579}, abstract = {Cellulose nanocrystals (CNC) are new class of cellulose materials that find wide applications in various research areas over the past two decades. These nanoparticles are usually made by acid hydrolysis of cellulose substances such as wood, cotton, Starch etc. The main aim of this study is to find the optimal conditions for obtaining an aqueous stable colloid suspension of cellulose nanocrystal (CNC) from α-cellulose with a high-yield procedure. Therefore various conditions of acid hydrolysis were evaluated as reaction temperature and reaction time. The percentage of yield was calculated for all suspensions. The morphology of the prepared CNC was characterized by Transmission Electron Microscopy (TEM), Environmental Scanning Electron Microscopy (ESEM) and the crystallinity was measured by X-ray diffraction (XRD). The results showed that highest yield of CNC (88%), was achieved from the reaction condition of 60 minutes at 60 °C. Generally, rod-like shape crystals achieved from α-cellulose with an average size of 35-50 nm and high crystallinity (92%) can be make it to a convenient and competitive source for the production of cellulose nanocrystal for various industries.}, keywords = {CELLULOSE,Cellulose Nanocrystal,α-Cellulose,Acid hydrolysis,yield,optimal conditions}, title_fa = {تهیه نانوکریستال سلولز از آلفا سلولز و بهینه سازی شرایط ساخت آن}, abstract_fa = {نانوکریستال سلولز (CNC) گروه جدیدی از مواد سلولزی است که طی دو دهه اخیر در حوزه‌های تحقیقاتی گوناگون کاربردهای وسیعی یافته است. این نانو ذرات اغلب از طریق هیدرولیز اسیدی ترکیبات سلولزی از قبیل چوب، پنبه، نشاسته و ... تهیه می‌شوند. هدف اصلی این تحقیق، یافتن شرایط بهینه برای ساخت سوسپانسیونی کلوئیدی پایدار در آب از نانوکریستال سلولز حاصل از آلفا سلولز طی روشی با بازدهی بالا می باشد. بنابراین شرایط متفاوتی از دما و زمان واکنش برای هیدرولیز اسیدی انتخاب شد. درصد بازده برای تمام سوسپانسیون‌های حاصل محاسبه گردید. ریخت شناسی نانوکریستال سلولز تهیه شده با استفاده از میکروسکوپ الکترونی عبوری (TEM) و میکروسکوپ الکترونی روبشی محیطی (ESEM) مورد بررسی قرار گرفت و کریستالیته با استفاده از پراش پرتو ایکس (XRD) اندازه‌گیری شد. نتایج نشان داد که بیشترین بازده نانوکریستال سلولز (88 درصد) در زمان 60 دقیقه و دمای 60 درجه سانتی گراد به دست آمد. به طور کلی، کریستال‌های میله‌ای شکل به دست آمده با ابعاد 50-35 نانومتر و کریستالیته بالا (92 درصد) از آلفا سلولز می‌تواند آن را به منبعی مناسب و رقابتی برای تولید نانوکریستال سلولز مورد نیاز صنایع مختلف مبدل سازد.}, keywords_fa = {سلولز,نانوکریستال سلولز,آلفا سلولز,هیدرولیز اسیدی,بازده,شرایط بهینه}, url = {https://ijwpr.areeo.ac.ir/article_109579.html}, eprint = {https://ijwpr.areeo.ac.ir/article_109579_4852bc5a90201e45e36a62de20c77a94.pdf} }