In this research the effect of nail′s length on three different values (32,42,48 mm)the nail number (2 and 3)and the kind of of particleboard and MDF on tensile strength and bending moment has been analyzed ,The member dimension of of 10*15*1.6 cm.have been elected for making of L –type joint. The junction have not used out of any adhesive as an adjuvant. From combination of this variable factors and examination of any strength some 24 samples have created,that due to the 4 iterations,96 specimens of L shaped joints have been coustructed totally.the bending and tensile strength of produced junction has been measured by mechanical test machine.based on captured results the interaction of constituents of,nail penetration length,nails number and members nature on joint strenght weren′t significant in front of tensile and bending.this research indicated that the junctions with the penetration length of 48 mm,the most amount of nail(three nails)on MDF member elements,have the greatest strength against bending strength,and the link with penetration length of 42mm alone with the most amount of nail(3 nails)on MDF have the greatest strength against tensile,as copared with each other.
Keywords